Title: The combinable precast

Author(s): Burón Maestro, M.; Fernández-Ordoñez Hernández, D.; Gómez Sanz, L.

Publication: ACHE

Volume: 48

Issue: 203

Appears on pages(s): 53 - 62

Keywords:

DOI:

Date: 1/1/1997

Abstract:
Actually, the precast industry offers the ""Combinable Precast"" as an efficient and competitive way of building, freely combining precast members. The technical properties, the performances and a proper use based on the dimensional coordination (modulation), of Combinable Precast is showed.