Title: Construction process of the 'Constitución de 1812' cable stayed Bridge over the Cadiz Bay

Author(s): Lucas Serrano, C.; Martínez Cutillas, A.; Navarro González-Valerio, J. A.

Publication: ACHE

Volume: 67

Issue: 278

Appears on pages(s): 101 - 109

Keywords: Construction sequence; Cable-stayed deck; Balanced cantilever; Segment

DOI:

Date: 1/3/2016

Abstract:
Balanced cantilever method has been use to erect the cable-stayed section of the Constitución de 1812" bridge over Cadiz Bay. Standard segments are 20 m long and 34 m width and weigh 4.000 kN.The construction sequence has been determined by the ultimate resistance of the tower that must resist the unbalanced bending moments at both sides of the tower."