Composite materials for building and public works. Cementious materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Composite materials for building and public works. Cementious materials

Author(s): Sánchez Gálvez, V.; Sánchez Paradela, M.L.

Publication: ACHE

Volume: 43

Issue: 183

Appears on pages(s): 109 - 118

Keywords:

DOI:

Date: 1/3/1992

Abstract:
Composite materials are produced by the combination of two different materials to achieve optimal properties. Among them, fober reinforced composites are increasingly used for buildings and public works, both with cementious matrices (FRC) and with polymer matrices (FRP). This first paper analyzes the properties, production methods and main applications of Fiber Reinfoced Cements and Concretes and particularly of Steel Fiber (SFRC), Glass Fiber (GRC), Polypropylene Fiver and Carbon Fiber (CRFC). In a next paper, a similar analysis of Fiber Reinforced Polymers (FRP) will be presented.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »