Measurement of thermal action in a solid slab concrete bridge deck and comparison to Eurocode 1 formulations

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Measurement of thermal action in a solid slab concrete bridge deck and comparison to Eurocode 1 formulations

Author(s): Corres Peiretti, H.; Ezeberry Parrotta, J. I.; Berecibar Oregui, A.; Pérez Caldentey, A.

Publication: ACHE

Volume: 63

Issue: 265

Appears on pages(s): 67 - 82

Keywords: uniform temperature, temperature gradient, concrete bridges, assessment, IAP-11, Eurocode 1, monitoring.

DOI:

Date: 1/5/2012

Abstract:
Continuous and extensive temperature readings obtained during a period of 3 years in an integral solid slab prestressed concrete bridge deck are presented. There are few experimental results for this type of concrete bridge deck. The measured values are then compared to predictions made using the formulation for temperature actions proposed by Eurocode 1.