Roig Gully Aqueduct

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Roig Gully Aqueduct

Author(s): Rueda Rieu, A.; Carbonell Cerezo, L.; Monzó Enguix, R.; Pastor Villanueva, J. M.; Ferreras Camarero, D.

Publication: ACHE

Volume: 62

Issue: 261

Appears on pages(s): 45 - 53

Keywords: aqueduct, pipe flow, stayed structure, tie rods, curved bars.

DOI:

Date: 1/5/2011

Abstract:
Despite the pressurized water pipe flow has got a higher flexibility in its course than the free surface flow, the terrain enforces the construction of auxiliary elements which allow the water transferring. In E stretch of the Jucar river down course connection with V stretch (Nueva conducción Júcar-Vinalopó") the pipe must overcome different transport infrastructures and four ravines, choosing pipe jacking and aqueducts respectively. This article is focused on the solution given to these aqueducts, especially to the Roig´s gully aqueduct, near the village of Moixent, for which conditions of various kinds imposed a unique design."


ACI International Partner, ACHE Spain, International Partner Access

View Resource »