Ductility and predictability in reinforced concrete sections

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ductility and predictability in reinforced concrete sections

Author(s): Puigdomènech Franquesa, L

Publication: ACHE

Volume: 54

Issue: 227

Appears on pages(s): 39 - 42

Keywords:

DOI:

Date: 1/1/2003

Abstract:
Ductility in reinforced concrete sections under bending situations is a welcome property for the Ultimate Limit States (aparent cracking and huge deformation for nearby collapse). Nevertheless, predictability is a related property with ductil sections, specially interesting for doubtly execution or variable concrete properties (i.e. recycled aggregates). This paper aims to developing a theoretical justification for the case of bending rectangular sections and expressions for estimating variability of moment in diferent designs. This is a humble contribution to work done by the Joint Committe on Structural Safety (JCSS).


ACI International Partner, ACHE Spain, International Partner Access

View Resource »