A study of the begaviour of concrete slab bridges under the environmental thermal effects. Design criteria

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A study of the begaviour of concrete slab bridges under the environmental thermal effects. Design criteria

Author(s): Mirambell Arrizabalaga, E.; Aguado de Cea, A.

Publication: ACHE

Volume: 38

Issue: 163

Appears on pages(s): 65 - 106

Keywords:

DOI:

Date: 1/3/1987

Abstract:
En el presente artículo se analiza, de forma paramétrica, la influencia de diversas variables climatológicas, físicas, geométricas y de emplazamiento, sobre la respuesta técnica de los tableros de puentes losa de hormigón, mostrándose, por una parte, la correlación existente entre el rango anual de la temperatura ambiente en el lugar de emplazamiento del puente y el rango anual de la temperatura media de este y, por otra, la correlación existente entre la intensidad de radiación solar incidente sobre el tablero del puente y el gradiente térmico vertical al que este se ve sometido. Asimismo, se presenta una metodología general de obtención de las acciones térmicas que se deben considerar en el diseño de puentes de hormigón. Dicha metodología se aplica al caso de puentes losa maciza y losa aligerada, emplazados en la geografía de nuestro país. Los resultados referentes a las acciones térmicas de diseño, derivados del presente estudio, se analizan comparativamente con los obtenidos mediante la aplicación de la normativa nacional vigente.