Compoasite materials in building and engineering. II. Materials with polymeric matrix

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compoasite materials in building and engineering. II. Materials with polymeric matrix

Author(s): Sánchez Gálvez, V.; Sánchez Paradela, M.L.

Publication: ACHE

Volume: 43

Issue: 184

Appears on pages(s): 115 - 123

Keywords:

DOI:

Date: 1/5/1992

Abstract:
Fiber Reinforced Polymers (FRP) are being increasingly used in Building and Civile Engineering. Among them, the most widely used material is Glassfiber Reinforced Polyester (GRP). In this paper, different production methods of GRP are presented as well as the mechanical properties achieved. On the other hand, main utilisations of FRP in Building and Civil Engineering are also shown, their advantages and disadvantages compared to traditional materials being analyzed.