Title: Conclusions and innovations applied

Author(s): Barceló Llauger, J.; Troya Gozálvez, L.; Peset González, L.

Publication: ACHE

Volume: 53

Issue: 226

Appears on pages(s): 175 - 180

Keywords:

DOI:

Date: 1/8/2002

Abstract:
In summary, these are pioneering works in the field of structural concrete. A brief history of the evolution of maritime concrete structures is given. A forecast is also made of possible future trends in port, urban and industrial developments. Another advantages are: building far from the final place of use is the environmental factor, as well as the revolutionary massive use of pre-stressing in this field. Finally, details are given of all the innovations involved in this project, from its original conception and design to the materials used and processes applied.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »