Analytical interpretation of Branson's formula for the calculation of deflections in reinforced concrete members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analytical interpretation of Branson's formula for the calculation of deflections in reinforced concrete members

Author(s): Marí Bernat, A.R.; Mirambell Arrizabalaga, E.; López Almansa, F.

Publication: ACHE

Volume: 41

Issue: 174

Appears on pages(s): 61 - 66

Keywords:

DOI:

Date: 1/1/1990

Abstract:
In this paper a theoretical study about deformations in reinforced concrete beams is presented. The beams have similar characteristics to those considered by Branson to obtain the equivalent inertia. In this study the deformation of the beam is simulated by a mathematical model taking into account cracking. An expression for the equivalent inertia for the calculation of deflections in reinforced concrete cracked beams which is very similar to the one obtained by Branson has been obtained.