Prefabricated structural systems for the construction of large span framed sheds

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prefabricated structural systems for the construction of large span framed sheds

Author(s): Atienza Reales, J.R.; López Desfilis, V.J.; Irles Más, R.; Codina Llopis, J.M.

Publication: ACHE

Volume: 40

Issue: 171

Appears on pages(s): 59 - 62

Keywords:

DOI:

Date: 1/3/1989

Abstract:
In this paper the structure and the constructive process of a framed shed built with prefabricated concrete elements is described. The elements that form the main supporting structure, reinforced concrete hinged portal frames, are the most remarkable. These portal frames cover a span of 45 m, the cross-section being a variable depth double T, and they are spaced 15 m. The three different pieces that make the frame (around 30 t each) are assmebled ""in ditu"" in the point of the lintel where the bending moment is minimum.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »