Thermal movements of joints and bearing systems on concrete bridges located on the Iberian Peninsula

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Thermal movements of joints and bearing systems on concrete bridges located on the Iberian Peninsula

Author(s): Mirambell Arrizabalaga, E; Aguado de Cea, A.; Aparicio Bengoechea, A.C.

Publication: ACHE

Volume: 39

Issue: 168

Appears on pages(s): 22-Sep

Keywords:

DOI:

Date: 1/5/1988

Abstract:
In this paper, a general methodology for the design of joints and bearing systems of concrete bridges located on the Iberian Peninsula is presented. Such methodology takes into account the longitudinal movements induced by envoironmental thermal effects. Design recommendations which allow to accurately predict thermal movements, depending on the location of the bridge, the cross section type and other factors which influence significantly the thermal response of the bridge, are presented.