Precast structures for multistory buildings achieved with rigid joint frames

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Precast structures for multistory buildings achieved with rigid joint frames

Author(s): Burón Maestro, M.; Fernández-Ordóñez Hernández, D.; Gómez Sanz, L.

Publication: ACHE

Volume: 46

Issue: 196

Appears on pages(s): 97 - 101

Keywords:

DOI:

Date: 1/3/1995

Abstract:
It is shown an example of a structure of six levels built with reinforced concrete and prestressed concrete elements, precast in the factory (beams, columns and deck slabs), placed and fixed together on site to form real rigid joint frames. It is achieved thus a rigid joint frame structure, able to resist horizontal forces. This permits us to avoid the construction of shear walls in the building.