Umbraced structures in reinforced concrete. Second order deformations

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Umbraced structures in reinforced concrete. Second order deformations

Author(s): Bernárdez, R.

Publication: ACHE

Volume: 40

Issue: 172

Appears on pages(s): 41 - 57

Keywords:

DOI:

Date: 1/5/1989

Abstract:
It is shown in this article the calculation of structures considering the second order deformations. Fistly, the simplified methods to study the buckling of isolated structural members are revised. The matrix calculation of structures by means P-Delta analysis is shown in a simplified version and in a more accurate one, that uses the diagrams of materials. Finally an alternate method is presented. It is a method that, considering the second order deformations of an isolated member, consideres as well the constraints that the whole structure makes over it.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »