Confinement of RC square columns using prefabricated composite jacketing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Confinement of RC square columns using prefabricated composite jacketing

Author(s): Perera Valemazán, R.; Recuero Forniés, A.; de Diego Villalón, A.; López Hombrados, C.

Publication: ACHE

Volume: 56

Issue: 235

Appears on pages(s): 43 - 52

Keywords:

DOI:

Date: 1/1/2005

Abstract:
Jacketing of reinforced concrete columns enhances their strength and ductility. This method, therefore, makes possible the repairing or retrofitting of existing columns in which the conditions have changed in relation to the original design. Usually, steel jackets have been used. However, in recent years, composite jackets have been used increasingly. This material has many advantages which make attractive its use as it has been checked for circular columns. However, for square columns the effectiveness is not so evident. In order to verify this, some compression tests and some numerical studies have been performed on square reinforced concrete columns strengthened using prefabricated fibre-reinforced polymer jackets.The results are presented in this paper.