La Vicaría arch bridge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: La Vicaría arch bridge

Author(s): Pérez-Fadón Martínez, S.; Herrero Beneítez, J. E.; Martín-Tereso López, L.

Publication: ACHE

Volume: 61

Issue: 255

Appears on pages(s): Jul-41

Keywords: Bowstring arch, composite bridge, Cor-ten steel, self-consolidating concrete, hoisting, hangers.

DOI:

Date: 1/1/2010

Abstract:
La Vicaria Bridge is a half-through arch viaduct with a composite deck. It crosses La Fuensanta, a reservoir in the Spanish province of Albacete fed by the Segura River. The viaduct?s two arches, each positioned on one side of the deck, span 168 m of its total 260-m length. Both slant inward at a 10º angle. The quasi-rectangular arch sections consist of folded steel plates filled with self-consolidating concrete, while the deck comprises two longitudinal steel trough girders connected by a concrete slab. The construction procedure used was to assemble the 120-m bowstring arch on the reservoir bed first and then hoist it into place 40 m above ground level with hydraulic jacks. It was subsequently joined to the rest of the bridge members built to cantilever from the two banks.