Technological innovations: road and paving durables and cheaps. Main sewers of concrete ""in situ"" with slide form

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Technological innovations: road and paving durables and cheaps. Main sewers of concrete ""in situ"" with slide form

Author(s): Vázquez Ruiz del Arbol, J.R.

Publication: ACHE

Volume: 47

Issue: 201

Appears on pages(s): 115 - 126

Keywords:

DOI:

Date: 1/5/1996

Abstract:
New constructive systems are presented in this paper. They consist in the realization of paving that remain interlaced by rugose and inclined surfaces made from the natural fissure of the concrete. This avoids the ""pumping"" and allows long life at the paving. Also, in this paper, is described lightened paving to let save concrete in a 30% and it is not necessary formworks using slide forms. The main sewers of concrete ""in situ"" made by the continuous method on the ground, is another of the applications using a system like the other one commented before. All these systems make good use of the characteristics of the matherials, with a geometry appropiated in roads, and taking account the earth pressure in the case of main sewers.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »