The ""Paste efficiency"" concept. It's application to estimate in situ the strength of hardened concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The ""Paste efficiency"" concept. It's application to estimate in situ the strength of hardened concrete

Author(s): Hostalet Alba, F.

Publication: ACHE

Volume: 48

Issue: 203

Appears on pages(s): 33 - 47

Keywords:

DOI:

Date: 1/1/1997

Abstract:
One of the more controversial application and, in spite of that, more used of the ultrasonic pulse method is the estimation of in situ concrete strength, if we atke into account the number of variables which can influence the results obtained in the test. The international normative and reccomendations, hence the spanish norme UNE, show that is neccesary to obtain specific calibrations between ultrasonic pulse velocity and concrete strength for every concrete under examination. The ""Paste efficiency"" concept, from H. N. Tomsett, based in the pulse velocity difference between a control specimen and the concrete in the structure, can be used to estimate the air-dried samples strength and hence in situ concrete strength. This paper presents an experimental research that has been developed under concrete which is normally placed in prestressed beams made in a central factory. The aims of this research has been to verify the application of the ""Paste efficiency"" concept, and levels of accuracy that we can achieve in estimating in situ hardened concrete strength placed in real prestressed beams, by means of ""Paste efficiency"" concept.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »