Title: Precast prestressed bridges. Recent achievements

Author(s): Burón Maestro, M.; Fernández-Ordóñez Hernández, D.; Peláez Ruiz, M.

Publication: ACHE

Volume: 45

Issue: 192

Appears on pages(s): 123 - 126

Keywords:

DOI:

Date: 1/5/1994

Abstract:
Several construction examples of Precast Prestressed multiple span bridges are shown. Built with box beam elements, prestressed in the factory and later connected with each other by means of an external prestressing, thus forming a multiple span bridge. Constant and variable depth bridge examples are shown.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »