The materials in the Eurocode 4

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The materials in the Eurocode 4

Author(s): Valiente Cancho, A.; Navarro Ugena, C.

Publication: ACHE

Volume: 43

Issue: 185

Appears on pages(s): 17 - 27

Keywords:

DOI:

Date: 1/8/1992

Abstract:
The behaviour of structural materials, as considered in EC4 for composite steel and concrete structuers, is analyzed in this work. The mechanical and thermomechanical models assumed by the eurocode for concrete and steel are reviewed, as well as the material properties ffrom which the models are cuantitatively characterized.