Title: The precast concrete in the old bridges rehabilitation. Decks and archs

Author(s): Burón Maestro, M.; Fernandez-Ordoñez Hernandez, D.

Publication: ACHE

Volume: 47

Issue: 200

Appears on pages(s): 63 - 71

Keywords:

DOI:

Date: 1/3/1996

Abstract:
The bridges rehabilitation adapts the old structures to the news functional needs. In cases of the old steelwork or reinforced concretework decks, the sustitution is necessary. The use of precast concrete elements permits: to reduce the deck weight increment, using high-strength concrete. To shorten the rehabilitation time. To fit the erection process in the useful parts of the old structure. To resolve with precission and strict geometry the bearing and connection details. As an example, the rehabilitation of a 1930s bridge with four spans of 32m built according to the Official Models of Arch Bridges by Mr. Jose Ribera is described. The precast technology allows to adapt many old bridges to the news traffic and security needs.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer