Caixa Forum building in Zaragoza

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Caixa Forum building in Zaragoza

Author(s): Brufau Niubó, R.; Bretón Brat, C.; Pierantoni Silva, F.; Guillén Angulo, D.

Publication: ACHE

Volume: 66

Issue: 277

Appears on pages(s): 191 - 201

Keywords: Large cantilevers; Climbing formwork; Fusiform composite support; Great depth trusses; Solid slabs; Composite metal deck slab; Self- compacting concrete

DOI:

Date: 1/5/2015

Abstract:
The CaixaForum building in Zaragoza, a project by Carme Pinós Studio, houses an auditorium, different exhibition halls, multipurpose spaces, and several lecture rooms. Its architecture, with a strong sculptural character, required a variety of unique structural solutions. The building is conformed as two cubes hung from a central communication core, both of them partially cantilevered. The main structural elements are the concrete walls supporting part of the cubic volumes, which are made up using large trusses and floor slabs of composite metal plates. The whole stability is achieved by the weight of the 40 cm solid slabs of the vertical communication core, which the two unobstructed spaces share.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »