Temporary cofferdams for the marine foundations of the Constitucion de 1812 Bridge over the Cadiz Bay

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Temporary cofferdams for the marine foundations of the Constitucion de 1812 Bridge over the Cadiz Bay

Author(s): González Barcina, J. M.; Niño Tejedor, F.; Bernardo Gutiérrez, H.; Jiménez Aguadero; V.M.

Publication: ACHE

Volume: 67

Issue: 278

Appears on pages(s): 37 - 42

Keywords: Cofferdams, Foundations, Marine work, Steel structure, Composite structure

DOI:

Date: 1/3/2016

Abstract:
The foundations of 10 piers of the new 1812 Constitution Bridge over the Cadiz Bay are located in the sea. They consist of long reinforced concrete piles below large pile caps of the same material. Pile shafts have been constructed using temporary metal sheets previously driven into the seabed. Dry construction of the pile caps has required the use of unique temporary steel cofferdams specially designed for this worksite. This paper describes these cofferdams, together with their key design and construction features.