Title: Gor river Bridge

Author(s): Ayala, E,J.; Creus, J.M.

Publication: ACHE

Volume: 45

Issue: 192

Appears on pages(s): 107 - 116

Keywords:

DOI:

Date: 1/5/1994

Abstract:
The Gor River Bridge is located in the A.92 Highway, between Guadix and Baza cities. It crosses the walley 85 m high. Different alternates were compares at the preliminary studies. A segmental prestressed concrete box girder bridge was finally selected. Twin decks of 600 m radius, with 3,50 m depth, were launched from an abutment. A forward steel nose was used. Total length of the bridge is 388 m, divided into 6 internal spans of 52 m and end spans of 38 m. This paper deals with the most interesting aspects of the preliminary studies, final design and construction of the bridge, with particular incidence on singularities.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »