Iberdrola Tower, Abandoibarra, Bilbao. Foundations and structure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Iberdrola Tower, Abandoibarra, Bilbao. Foundations and structure

Author(s): Mayo Martínez, María del Mar

Publication: ACHE

Volume: 64

Issue: 269

Appears on pages(s): 31 - 46

Keywords: high rise building, diaphragm walls constructed by hydrofraise system, diaphragm anchors below the water table, water uplift slab, postensioned foundation, differential shortening, concrete slabs.

DOI:

Date: 1/5/2013

Abstract:
The Iberdrola Tower is part of the urban projects developed for the Nervion riverside recovery in the city of Bilbao, and is located within the former industrial area known as Campa de los Ingleses" in Abando-Ibarra, joining the nearby Guggenheim museum as a new landmark. It is a 165 meters above ground construction, including 40 floors above ground and up to 5 parking floors under ground, adding up to 190 meters. Upon completion, it surpassed the BEC tower height by 65 meters, becoming the tallest building in Biscay and ranking eighth in Spain."