Mengibar bridge over the Guadalquivir river in the motorway Bailén-Jaén (composite 100 m central span)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mengibar bridge over the Guadalquivir river in the motorway Bailén-Jaén (composite 100 m central span)

Author(s): Martínez Calzón, J.

Publication: ACHE

Volume: 50

Issue: 211

Appears on pages(s): 63 - 70

Keywords:

DOI:

Date: 1/1/1999

Abstract:
The must important feature of this two cell box girder bridge with double composite action is the unique geometric solution and erection method for the concrete deck slab of the structure. This slab have a orthotropic rib system which permits a very simple semiprecast erection procedure without any type of formworks. With this achievement the total construction of the deck once finished the self-resistant steel structure was an absolute minimum


ACI International Partner, ACHE Spain, International Partner Access

View Resource »