Aconcrete and steel challenge: Normandy bridge, world record cable stay span

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Aconcrete and steel challenge: Normandy bridge, world record cable stay span

Author(s): de la Fuente, C.

Publication: ACHE

Volume: 44

Issue: 188

Appears on pages(s): 81 - 104

Keywords:

DOI:

Date: 1/5/1993

Abstract:
The Normandy bridge, cable-stayed structure with 856 m main span, is one of the world's largest civil works under construction. The author describes in this paper the entire projrct as a whole, detailing also some design features, in particular those related with post-tensioning and cable stays. The description reflects the present status of the works as well as the various solutions adopted to solve the problems arisen by the size of this project.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »