Theoretical and experimental investigation on the begabiour of post-tensioned flat slabs with unbonded tendons. Objectives, description of tests and previous stuctural analysis

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Theoretical and experimental investigation on the begabiour of post-tensioned flat slabs with unbonded tendons. Objectives, description of tests and previous stuctural analysis

Author(s): Marí Bernat, A.R.; Murcia Vela, J.; Roca Fabregat, P.; Vives Escuder, A.; Adell Torrelles, J.C.

Publication: ACHE

Volume: 41

Issue: 177

Appears on pages(s): 131 - 141

Keywords:

DOI:

Date: 1/8/1990

Abstract:
The purpose of this paper is to presnt the objectives ot the theoretical and experimental research project on ""Flat slabs with unbonded tendons"", which is currently being debeloped at the ETSICCP of Barcelona, as well as to present the experimental program which is planned to be carried out. A description of the first specimen consisting on a slab of 10m x 8m x 0,14 m supported on 9 columns is made, explainng the criteria used for its design, construction, loading and measuring systems, as well as the specific characteristics of the laboratory where the tests are being carried out. Some comments relative to the analytical modem used to predict the experimental results are also made.