High strength concrete. Reciongal experience. Cordoba. Argentina

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High strength concrete. Reciongal experience. Cordoba. Argentina

Author(s): Durán, G.; Cuneo Simian, H.

Publication: ACHE

Volume: 43

Issue: 183

Appears on pages(s): 79 - 99

Keywords:

DOI:

Date: 1/3/1992

Abstract:
The purpose of this paper is to study a type of high strength concrete made with regional materials and using conventional technics. Correlation of the properties of mortar and rock with concrete strength was included regarding: mix design, handling, placing and strength. A methodology was developed which permit a variational mix design. Experimental work includes 72 concrete cylindric specimens (150 x 300 mm), 48 mortar prismatic specimens (160 x 40 x 40 mm) and rock specimens. Mechanical properties were evaluated for different ages. The parameters included were: compressive and flexural strength, modulus of elasticity and ultrasonic pulse velocity. These properties were evaluated for the concrete, the mortar and the rock.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »