Title: Patch repair evaluation of corroed reinforced concrete girders

Author(s): Río Suárez, O.I.; Alonso Alonso, M.C.; Andrade Perdrix, M.C.; Vega Catalán, L.

Publication: ACHE

Volume: 51

Issue: 217

Appears on pages(s): 101 - 109

Keywords:

DOI:

Date: 1/5/2000

Abstract:
The results of the experimental tests carried out in order to study the mechanical behaviour of bending elements are presented. Repaired and unrepaired concrete elements (girders) are considered. Previously, the elements were submitted to an accelerated local corrosion process, by chloride penetration. Both the structural behaviour and the efficiency of the repair system in the ULS and the SLS were checke