Comparative study on concrete permeability limits in Spanish and European standards

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparative study on concrete permeability limits in Spanish and European standards

Author(s): Gálligo Estévez, J.M.; Rodríguez García, F.

Publication: ACHE

Volume: 46

Issue: 195

Appears on pages(s): 37 - 47

Keywords:

DOI:

Date: 1/1/1995

Abstract:
The Spanish Codes for concrete, EH-91 and EP-93, include at present procisions for limiting the permeability of concrete, measured in the water penetration test described in the UNE 83.304/90 standard. The prescriptios of the Spanish Codes are not exactly coincident with the ones of ENV-206. So, the limiting value for the average penetration depth is different: 20 mm for ENV-206 while 30 mm in the Spanish Codes. The broad experience in this field of the Laboratorio Central de Estructuras y Materiales from CEDEX, has allowed to perform a study on the validity of the average penetration depth fronts in both standards. In the study, both laboratory cast concrete samples, and in-suty drilled cores were used. In the paper, the study is described in general terms, and the main conclusions are presented, these revealing a higher soundness of the limiting values in the Spanish Codes. Also a study of the deviations obtained in the test is performed, and a procedure is presented for using the water penetration test as a standard control method for the durability specifications of concrete.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »