Arenal"" bridge at Córdoba

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Arenal"" bridge at Córdoba

Author(s): Martínez Calzón, J.

Publication: ACHE

Volume: 45

Issue: 192

Appears on pages(s): 117 - 122

Keywords:

DOI:

Date: 1/5/1994

Abstract:
The work is a continuous prestressed composite bridge with three spans at 55-110-55 m with many variable sections. The bridge includes in the central supports semiactive devices with vertical bars acting as tendons anchorages to the piers, that fix favourably the central span, improving its slenderness without damage for the lateral spans. The bridge is enclose in a typological line developed by the author in other very important previous works. In this previous works large prestressed concrete elements are inserted in a continuous way with box girders with double composite action. In this bridge the steel-concrete blend is fully interactive and achieves a deep structural and visual continuity between all the materials and the different cross sections.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »