Designing deck-point of fixity connections

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Designing deck-point of fixity connections

Author(s): Crespo Martínez, J. A.; Lorenzo Esperante, D.; González de Cangas, J. R.

Publication: ACHE

Volume: 62

Issue: 260

Appears on pages(s): 47 - 60

Keywords: fixed point, anchoring, connection, prestressed slab, precast beams, box girder.

DOI:

Date: 1/3/2011

Abstract:
This article describes different typologies used in SILGA for the design of the connection of the deck to the fixed point to where forces due to traction, braking, and occasionally earthquake are transmitted. Aspects about its analysis, dimensioning and durability and maintenance oriented design are also covered.