Almonte Arch. La Plata dual carriageway. Hinojal-Cáceres stretch

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Almonte Arch. La Plata dual carriageway. Hinojal-Cáceres stretch

Author(s): Siegrist Ridruejo, G.

Publication: ACHE

Volume: 57

Issue: 240

Appears on pages(s): 29-May

Keywords:

DOI:

Date: 1/3/2006

Abstract:
This article describes the type and construction process involved in the Bridge over the River Almonte, on the Hinojal ? Cáceres Stretch of La Plata N-630 dual carriageway joining Gijón and Seville, whose construction concluded in 2005. The arches were built by combining the cantilever method with a powerful rigid rolled steel section triangulation which allowed for the tensioning of conventional rolled sections. The deck was built using scaffolding trusses from both ends and everything was real time monitored by efficient instrumentation that made use of state-of-the-art technology.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »