Enlargement of arch bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Enlargement of arch bridges

Author(s): Llombart Jaques, J.A.; Revoltós Fort, J.

Publication: ACHE

Volume: 46

Issue: 198

Appears on pages(s): 57 - 79

Keywords:

DOI:

Date: 1/8/1995

Abstract:
This article describes three different enlargements of short span arch bridges . In three bridges, the prefabrication of the elements of the deck has permited a quick and economical construction; avoiding in any case, the use of arch falsework which are always expensive. Moreover, under aesthetical point of view, the use of prefabricated elements has been made compatible with the shape of the existent deck in order to mantain the external appeareance.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »