Special anchorages for the new railway bridge over the river Duero in Oporto (Portugal)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Special anchorages for the new railway bridge over the river Duero in Oporto (Portugal)

Author(s): Ripoll, J.B.; Ayats Calsat, J.

Publication: ACHE

Volume: 40

Issue: 170

Appears on pages(s): 157 - 162

Keywords:

DOI:

Date: 1/1/1989

Abstract:
This article explains the technical reasons which have leaded to the design of a special anchorages. Also we have enclosed a description of these special anchorages, detailing their main features.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »