Torrelodones bridge over the Guadarrama river

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Torrelodones bridge over the Guadarrama river

Author(s): Fernández Troyano, L.; Manterola Armisén, J.

Publication: ACHE

Volume: 42

Issue: 180

Appears on pages(s): 81 - 84

Keywords:

DOI:

Date: 1/5/1991

Abstract:
This bridge substitutes a stone arch ehich was built by Juan de Herrera in the XVI Century for the road drom Madrid to El Escorial. The new bridge is also a tympan arch; it is hinged at the extremes and it is supported on two piramidal abutments.