Treatment of the prestressed concrete in athe "Eurocode 2"

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Treatment of the prestressed concrete in athe "Eurocode 2"

Author(s): del Pozo Vindel, F.J.; Marí Bernat, A.R.

Publication: ACHE

Volume: 43

Issue: 182

Appears on pages(s): 101 - 109

Keywords:

DOI:

Date: 1/1/1992

Abstract:
This paper contains a study of the treatment of the prestressed concrete in the Eurocode EC-2. The aim of the study is not to analyze exhaustively the subject but to pay particular attention to the most important themes and its differences and similitudes with the Spanish code EP-80.