Cable stayed footbridge, to access the intake tower of the Francisco Abellán Dam

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cable stayed footbridge, to access the intake tower of the Francisco Abellán Dam

Author(s): Llombart, J.A.; Revoltós Fort, J.

Publication: ACHE

Volume: 47

Issue: 201

Appears on pages(s): 81 - 94

Keywords:

DOI:

Date: 1/5/1996

Abstract:
This paper describes a cable stayed footbridge, built to access the intake tower of the Francisco Abellán Dam. The footbridge is a symmetric structure with two spans of 45,00 m each, and a composite box girder. The construction was done by launching the wall steel structure from one hillside, in order to avoid expensive lifting means due to high cliff.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »