How to repair a bridge's beam damaged

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: How to repair a bridge's beam damaged

Author(s): González Serrano, A.

Publication: ACHE

Volume: 42

Issue: 178

Appears on pages(s): 105 - 109

Keywords:

DOI:

Date: 1/1/1991

Abstract:
This paper explains how to repair a bridge's beam that was damaged by a strong impact of a tank truck. The impact in the edge's beam of a bridge crossing over the road in Betanzos, La Coruña.