Title: Foundations of the 'Constitución de 1812' Bridge over the Cadiz Bay

Author(s): Fernández Eusebio, A.; Pita Olalla, M.

Publication: ACHE

Volume: 67

Issue: 278

Appears on pages(s): 33 - 36

Keywords: Borehole, Ostionera, Pliocene, Bored pile/Drilled shaft, Pile cap, Sheet pile wall.

DOI:

Date: 1/3/2016

Abstract:
This paper includes a brief summary of the main geotechnical features of foundation's ground and of the geotechnical surveys that were performed to define them. It also includes a description of the main characteristics of the pile foundations and some of the ancillary means used during the construction of piles and pile caps.