Title: Cross-section design and verification in high-strength concrete columns and beams

Author(s): Morán Cabré, F.; Gutiérrez Jiménez, J. P.

Publication: ACHE

Volume: 61

Issue: 257

Appears on pages(s): 69 - 79

Keywords: reinforced concrete, RC Structures, High Strength Concrete, Design of RC cross-sections.

DOI:

Date: 1/5/2010

Abstract:
This paper presents numerical, dimensionless tables and approximate formulae for the design and checking of RC rectangular cross-sections of beams and columns made of High Strength Concrete (HSC). These tables and formulae are valid for HSC up to 100 N/mm2, and are based on the new parabola-rectangle stress-strain diagrams for HSC of the last issue of the Spanish RC Code EHE-08.