The influence of pearlite colony orientation on stress corrosion cracking of eutectoid steels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The influence of pearlite colony orientation on stress corrosion cracking of eutectoid steels

Author(s): Lancha, A.M.; Elices Calafat, M.

Publication: ACHE

Volume: 39

Issue: 167

Appears on pages(s): 143 - 151

Keywords:

DOI:

Date: 1/3/1988

Abstract:
This paper presents results on stress corrosion cracking of two eutectoid steels for prestressing concrete; before and after cold drawing. Tests have been performed on precracked specimens axially loaded (Slow Strain Rate Test). The regimes of environment sensitive fracture were detected. The high potential regime is sensitive to cold drawinf differences. The lower potential regime of cracking is similar for both wires (before and after cold drawing).