Abstract:
This paper presents the final results of ""Working Group for Handbook of Mantienance of Prestressed Bridges HP-7"", which labour has been developed during th last years. The Handbook extends the duration of the HP-6 Handbook for the specific case of prestressed bridges, with the same orientation and aim.