Theoretical and experimental study on the shear behaviour of dry joints segmental bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Theoretical and experimental study on the shear behaviour of dry joints segmental bridges

Author(s): Ramos Schneider, G.; Aparicio Bengoechea, A.C.; Turmo Coderque, J.; Polo Orodea, T.; Piernagorda Pardàs, J.; Llopart Martínez, S.

Publication: ACHE

Volume: 55

Issue: 232

Appears on pages(s): 51 - 61

Keywords:

DOI:

Date: 1/3/2004

Abstract:
This paper presents the research project PB98-0927 supported by the Spanish Ministry of Education and Culture from 1999 to 2002. This project included extensive testing and numerical modelling of the behaviour on combined flexure and shear ultimate limit state of dry joints of segmental concrete bridges.