Various prestressed bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Various prestressed bridges

Author(s): Granell Vicent, I.

Publication: ACHE

Volume: 40

Issue: 170

Appears on pages(s): 33 - 63

Keywords:

DOI:

Date: 1/1/1989

Abstract:
This report sets out the main features, from a point of view of design and construction, of the structures that belong to the following works: - Railway bridge over the Manzanares River and M-30, belonging to the Atocha-Villaverde (Madrid) section, and consisting of two twin bridge decks with five spans of 25, 37,37,25 m of cleareance respectively. - Bridge belonging to the Kukularra Interchange, corresponding to the point where two branches cross over the Ugaldebieta mainline, forming a three-level intersection (Bilbao). These are two bridges with significant curvatures in plan, having a bicellular caisson cross-section, and with spans of 30,42 and 30 m and 20,32,20 m of cleareance respectively. - Bridges across the rotary that forms the intersection of CN-II with GE-533 and GE-672 (Gerona). These are two structures with two spans, having 38,5 and 18 m of cleareance respectively, with the compensating span forming part of the corresponding access-embankment. - Bridge over the Guadalquivir River, corresponding to the point where CN-321 crosses over said river in the place known as Puente del Obispo (Jaen). It consists of a structure of three spans with 45, 90 and 45 m of cleareance respectively, constructed by the cantilever method.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »