Ultra high performance fiber reinforced concrete (UHPFRC): innovations in one-way slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ultra high performance fiber reinforced concrete (UHPFRC): innovations in one-way slabs

Author(s): Camacho Torregrosa, E.; Serna Ros, P.; López Martínez, J. A.

Publication: ACHE

Volume: 63

Issue: 264

Appears on pages(s): 81 - 92

Keywords: back analysis, one way spanning, fibre orientation, precast, UHPFRC.

DOI:

Date: 1/3/2012

Abstract:
This study provides the design, calculation, casting and testing of a one-way spanning system made of self-compacting UHPFRC. It is composed of precast thin double T girders and thin flat slabs. Material was cast both at laboratory and at precast company, analysing the mechanical properties evolution. Full scale beams were made at laboratory without prestressed steel, deducing the stress-strain tensile law of the material by flexural tests. Prestressed beams were elaborated in a precast company and tested to check the real behaviour of the element. Besides 20 mm thickness slabs were tested to evaluate the capacity of the secondary elements which complete the system.The advantages of the system proposed are explained, comparing it with the conventional solutions and detailing the span range where it can be used for building and civil engineering.