Title: A new way for repairing concrete structures, using shear connections

Author(s): González Serrano, A.

Publication: ACHE

Volume: 42

Issue: 178

Appears on pages(s): 99 - 104

Keywords:

DOI:

Date: 1/1/1991

Abstract:
This work contains a new way of repairing concrete structures, using shear connections like the ones used in composite beams. The novelity consists in emplying mortars with high resistance, up to 20000 psi. It allows to bind the shear connectors to the old concrete with ssmall lengths.