Diagnosis and evaluation of reinforced concrete construction submited to fire damage

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Diagnosis and evaluation of reinforced concrete construction submited to fire damage

Author(s): Delibes Liniers, A.

Publication: ACHE

Volume: 40

Issue: 172

Appears on pages(s): 83 - 98

Keywords:

DOI:

Date: 1/5/1989

Abstract:
This work contains a proposal for the inspection and experimental assessment of the damage produced by fire to concrete constructions. The proposal is based on the current knowledge on the fire-resistance of concrete structures. The proposal will be a basisfor the judgement of the re-serviceability conditions of the damaged members.