A method for removing the supports of a commercial building

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A method for removing the supports of a commercial building

Author(s): González Serrano, A.

Publication: ACHE

Volume: 42

Issue: 178

Appears on pages(s): 127 - 133

Keywords:

DOI:

Date: 1/1/1991

Abstract:
This work deals with the method of removing most of the supports of a big commercial building. The method also allows to remove the only one existing floor.